Basit öğe kaydını göster

dc.contributor.authorRona, Nergiz
dc.contributor.authorYenisey, Murat
dc.contributor.authorKucukturk, Gokhan
dc.contributor.authorGurun, Hakan
dc.contributor.authorCogun, Can
dc.contributor.authorEsen, Ziya
dc.date.accessioned2020-06-21T13:26:32Z
dc.date.available2020-06-21T13:26:32Z
dc.date.issued2017
dc.identifier.issn1883-1958
dc.identifier.issn2212-4632
dc.identifier.urihttps://doi.org/10.1016/j.jpor.2016.07.006
dc.identifier.urihttps://hdl.handle.net/20.500.12712/12536
dc.description38th Annual Conference of the European-Prosthodontic-Association -- SEP, 2014 -- Istanbul, TURKEYen_US
dc.descriptionCogun, Can/0000-0001-5045-2767; Gurun, Hakan/0000-0001-6189-6830en_US
dc.descriptionWOS: 000402346600009en_US
dc.descriptionPubMed: 27575994en_US
dc.description.abstractPurpose: The study determined (i) the effects of electrical discharge machining (EDM) on the shear-bond strength (SBS) of the bond between luting resin and zirconia ceramic and (ii) zirconia ceramic's flexural strength with the three-point bending (TPB) test. Methods: Sixty 4.8 mm x 4.8 mm x 3.2 mm zirconia specimens were fabricated and divided into four groups (n = 15): SBG: sandblasted + silane, TSCG: tribochemical silica coated + silane, LTG: Er:YAG laser treated + silane, EDMG: EDM + silane. The specimens were then bonded to a composite block with a dual-cure resin cement and thermal cycled (6000 times) prior to SBS testing. The SBS tests were performed in a universal testing machine. The SBS values were statistically analyzed using ANOVA and Tukey's test. To determine flexural strength, sixty zirconia specimens were prepared and assigned to the same groups (n = 15) mentioned earlier. After surface treatment TPB tests were performed in a universal testing machine (ISO 6872). The flexural strength values were statistically analyzed using ANOVA and Tukey's test (a = 0.05). Results: The bond strengths for the four test groups (mean SD; MPa) were as follows: SBG (Control), 12.73 +/- 3.41, TSCG, 14.99 +/- 3.14, LTG, 7.93 +/- 2.07, EDMG, 17.05 +/- 2.71. The bond strength of the EDMG was significantly higher than those of the SBG and LTG (p < 0.01). The average flexural strength values for the groups SBG (Control), TSCG, LTG and EDMG were 809.47, 800.47, 679.19 and 695.71 MPa, respectively (p > 0.05). Conclusions: The EDM process improved the SBS. In addition, there was no significant adverse effect of EDM on the flexural strength of zirconia. (C) 2016 Japan Prosthodontic Society. Published by Elsevier Ltd. All rights reserved.en_US
dc.description.sponsorshipEuropean Prosthodont Assocen_US
dc.description.sponsorshipOndokuz Mayis University Scientific Research Coordination [1904.10.010]en_US
dc.description.sponsorshipSupported by Ondokuz Mayis University Scientific Research Coordination by grant no. 1904.10.010.en_US
dc.language.isoengen_US
dc.publisherElsevier Ireland Ltden_US
dc.relation.isversionof10.1016/j.jpor.2016.07.006en_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectZirconia ceramicen_US
dc.subjectElectrical discharge machiningen_US
dc.subjectBonding strengthen_US
dc.subjectFlexural strengthen_US
dc.subjectGraphite powderen_US
dc.titleEffect of electrical discharge machining on dental Y-TZP ceramic-resin bondingen_US
dc.typeconferenceObjecten_US
dc.contributor.departmentOMÜen_US
dc.identifier.volume61en_US
dc.identifier.issue2en_US
dc.identifier.startpage158en_US
dc.identifier.endpage167en_US
dc.relation.journalJournal of Prosthodontic Researchen_US
dc.relation.publicationcategoryKonferans Öğesi - Uluslararası - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster