dc.contributor.authorCakmak, Fethiye
dc.contributor.authorKocak, Sibel
dc.contributor.authorKocak, Mustafa Murat
dc.contributor.authorElekdag-Turk, Selma
dc.contributor.authorTurk, Tamer
dc.date.accessioned2020-06-21T13:46:37Z
dc.date.available2020-06-21T13:46:37Z
dc.date.issued2015
dc.identifier.issn2528-9659
dc.identifier.issn2148-9505
dc.identifier.urihttps://doi.org/10.13076/TJO-D-15-00006
dc.identifier.urihttps://hdl.handle.net/20.500.12712/14331
dc.descriptionWOS: 000439315100003en_US
dc.description.abstractObjective: To evaluate initial shear bond strengths (SBSs) of ceramic brackets using either a self-etching primer (SEP) or the conventional method (CM) after intracoronal bleaching with sodium perborate and distilled water. Materials and Method: Eighty human incisors were divided into 4 groups according to bleaching and bonding procedures: group 1, bleaching was not applied and brackets were bonded with SEP; group 2, bleaching was not applied and brackets were bonded with the CM; group 3, intracoronal bleaching with sodium perborate was applied for 3 weeks and brackets were bonded with SEP; group 4, intracoronal bleaching with sodium perborate was applied for 3 weeks and brackets were bonded with the CM. The SEP (Transbond Plus) was applied as recommended by the manufacturer. After SEP application, ceramic brackets were bonded with light cure adhesive (Transbond XT). For the CM, the teeth were etched with 37% phosphoric acid. After etching, a thin uniform coat of primer (Transbond XT Primer) was applied and ceramic brackets were bonded with light cure adhesive (Transbond XT). The SBSs were measured after water storage for 30 days, after 1000 cycles of thermocycling between 5 degrees C and 55 degrees C. Bond failure location was determined with the adhesive remnant index (ARI). Results: For the SEP method, there was no significant difference between the SBS values of the bleaching and nonbleaching groups. Furthermore, for the CM, the SBS value of the nonbleaching group was not significantly different from that of the bleaching group. The SBS values of the SEP method presented significant differences from the SBS values of the CM (p < 0.001). The SBS values of the SEP application decreased with and without bleaching. ARI scores did not show any significant difference between the groups (p = 0.174). Conclusion: Intracoronal bleaching with sodium perborate and distilled water did not affect the SBS values of ceramic brackets.en_US
dc.language.isoengen_US
dc.publisherAves Press Ltden_US
dc.relation.isversionof10.13076/TJO-D-15-00006en_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectBond Strengthen_US
dc.subjectCeramic Bracketsen_US
dc.subjectIntracoronal Bleachingen_US
dc.subjectSelf-Etching Primeren_US
dc.titleComparison of Shear Bond Strengths of Ceramic Brackets Using Either Self-etching Primer or Conventional Method After Intracoronal Bleachingen_US
dc.typearticleen_US
dc.contributor.departmentOMÜen_US
dc.identifier.volume28en_US
dc.identifier.issue2en_US
dc.identifier.startpage48en_US
dc.identifier.endpage54en_US
dc.relation.journalTurkish Journal of Orthodonticsen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster