dc.contributor.authorCetinkaya, Burcu Ozkan
dc.contributor.authorKeles, Gonca Cayir
dc.contributor.authorAyas, Bulent
dc.contributor.authorAydin, Oguz
dc.contributor.authorKirtiloglu, Tugrul
dc.contributor.authorAcikgoz, Gokhan
dc.date.accessioned2020-06-21T15:23:50Z
dc.date.available2020-06-21T15:23:50Z
dc.date.issued2007
dc.identifier.issn1432-6981
dc.identifier.issn1436-3771
dc.identifier.urihttps://doi.org/10.1007/s00784-006-0087-7
dc.identifier.urihttps://hdl.handle.net/20.500.12712/20084
dc.descriptionWOS: 000244186100007en_US
dc.descriptionPubMed: 17111121en_US
dc.description.abstractGuided tissue regeneration is based on preventing the more rapidly proliferating epithelium from growing into the periodontal defect after surgical procedures incorporating barrier membranes. The aim of this study was to compare the proliferative activity of gingival epithelium using proliferating cell nuclear antigen (PCNA) as a marker of cell proliferation after surgical treatments with bioactive glass graft material and bioabsorbable membrane. Using split mouth design, 20 intrabony defects were randomly assigned treatments with bioactive glass (BG group) or bioabsorbable membrane (BM group). Gingival biopsies were taken at preoperative and postoperative 12 weeks. After histological processing, the number of the inflammatory cells was measured in hematoxylin and eosin-stained sections; PCNA expression was determined in immunohistochemically-stained sections. At postoperative 12 weeks, the number of the inflammatory cells was significantly decreased (p < 0.01), PCNA expression was significantly increased (p < 0.001) in both treatment groups compared to baseline data. There was no significant difference in PCNA expression between baseline values of two groups (p > 0.05), while at postoperative 12 weeks, increase in BG group was significantly greater than that in BM group (p < 0.001). These results suggest that epithelial cell proliferation is more prominent after treatment of intrabony defects with bioactive glass compared to the treatment with bioabsorbable membrane.en_US
dc.language.isoengen_US
dc.publisherSpringer Heidelbergen_US
dc.relation.isversionof10.1007/s00784-006-0087-7en_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectguided tissue regenerationen_US
dc.subjectbioactive glassen_US
dc.subjectbioabsorbable membraneen_US
dc.subjectlong junctional epitheliumen_US
dc.subjectproliferating cell nuclear antigenen_US
dc.titleComparison of the proliferative activity in gingival epithelium after surgical treatments of intrabony defects with bioactive glass and bioabsorbable membraneen_US
dc.typearticleen_US
dc.contributor.departmentOMÜen_US
dc.identifier.volume11en_US
dc.identifier.issue1en_US
dc.identifier.startpage61en_US
dc.identifier.endpage68en_US
dc.relation.journalClinical Oral Investigationsen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster