The effect of curing lights and modes on dentin bond strength of bulk-fill composites applied in different thickness

Date

2019

Author

Misilli, Tugba
Gonulol, Nihan
Cabadag, Ozge Gizem
Almasifar, Lena
Misilli, Umut

Metadata

Show full item record

Abstract

To investigate shear bond strength (SBS) to dentin of a conventional and three bulk-fill composites applied in different increment thickness and cured by mono- and multi-wave LED LCUs. Two hundred and fifty-two extracted sound human molars were prepared for SBS test. The teeth were divided into four groups according to the resin composites used. Conventional composite: Tetric N-Ceram (control); high-viscosity bulk-fills: Tetric N-Ceram Bulk Fill, X-tra Fil, and SonicFill. Each group was subdivided (n = 7) according to increment thickness (2, 4, and 6 mm) and cured by standard mode of a mono-wave LED or two different modes (standard and xtra power) of a multi-wave LED. The failure mode was stereomicroscopically determined at 40x magnification. Data were analyzed using Three-way ANOVA and further comparisons were assessed by Bonferroni's multiple comparison test. There were no significant differences within X-tra fil and Tetric N-Ceram Bulk Fill groups for any of the variables (p > 0.05). A significant decrease in SBS values with increase of layer thickness was observed for SonicFill and control groups. Also, curing mode had a significant effect on both composites at 6 mm thickness and standard mode of multi-wave LED caused the highest SBS value (p < 0.05). Adhesive failure was the most common fracture pattern especially at 6 mm thickness applications. Based on the results of this study, the bulk-fill composites can be safely applied in one-step with 4 mm increments, although the examined composites performed better at 2 mm thickness. The performance of the composites at 6 mm increment may show differences related to the curing lights and modes.

Source

Journal of Adhesion Science and Technology

Volume

33

Issue

20

URI

https://doi.org/10.1080/01694243.2019.1640174
https://hdl.handle.net/20.500.12712/10716

Collections

  • Scopus İndeksli Yayınlar Koleksiyonu [14046]
  • WoS İndeksli Yayınlar Koleksiyonu [12971]



DSpace software copyright © 2002-2015  DuraSpace
Contact Us | Send Feedback
Theme by 
@mire NV
 

 




| Policy | Guide | Contact |

DSpace@Ondokuz Mayıs

by OpenAIRE

Advanced Search

sherpa/romeo

Browse

All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsTypeLanguageDepartmentCategoryPublisherAccess TypeInstitution AuthorThis CollectionBy Issue DateAuthorsTitlesSubjectsTypeLanguageDepartmentCategoryPublisherAccess TypeInstitution Author

My Account

LoginRegister

Statistics

View Google Analytics Statistics

DSpace software copyright © 2002-2015  DuraSpace
Contact Us | Send Feedback
Theme by 
@mire NV
 

 


|| Policy || Library || Ondokuz University || OAI-PMH ||

Ondokuz Mayıs University, Samsun, Turkey
If you find any errors in content, please contact:

Creative Commons License
Ondokuz University Institutional Repository is licensed under a Creative Commons Attribution-NonCommercial-NoDerivs 4.0 Unported License..

DSpace@Ondokuz Mayıs:


DSpace 6.2

tarafından İdeal DSpace hizmetleri çerçevesinde özelleştirilerek kurulmuştur.